References
1. X3 UHMWPE maintains mechanical properties after accelerated oxidative aging. No statistical difference was found for Tensile Yield Strength, Ultimate Tensile Strength and Elongation as measured per ASTM D638 before and after exposure to ASTM F2003 accelerated aging (5 Atmospheres (ATM) of oxygen at 70ÂșC for 14 days). Tensile Yield Strength was 23.5 +/- 0.3 MPa and 23.6 +/- 0.2 MPa, Ultimate Tensile Strength was 56.7 +/- 2.1 MPa and 56.3 +/- 2.3 MPa and Elongation was 267 +/- 7% and 266 +/- 9% before and after accelerated oxidative aging, respectively.